Atmospheric atomic layer deposition of SnO 2 thin films with tin (ii) acetylacetonate and water
Title | Atmospheric atomic layer deposition of SnO 2 thin films with tin (ii) acetylacetonate and water |
---|---|
Author | |
Year of Publication |
2022
|
Journal |
Dalton Transactions
|
Volume |
51
|
Start Page |
9278
|
Issue |
24
|